Supply Iron-based superalloy powder iron alloy powder 3D printing powder 

 

category

Alloy grades and characteristics

Alloy number:

Stainless steel:304,316L,410L,15-5PH,17-4PH,2Cr13;

high-strength steel:A100,300M,30CrMnSiA,40CrMnSiMoVA;

Work die steel:18Ni300,H13,M2,M35,M42,T15,2030,S390

Iron Nickel alloy powder:Invar 36

Particle size:

0-20μm, 15-45μm, 15-53μm, 53-105μm, 53-150μm, 105-250μm

Morphology:

Spherical or nearly spherical

Appearance:

Grey

Package:

Aluminum bag,Vacuum packing

Application:

3D printing metal powder

Other applications:

powder metallurgy(PM), injection molding(MIM), spray painting(SP) etc.

 