Composition(percentage by mass)
 

Ni

Cr

Co

Ti

Al

Mo

Ta

Bal

14.0-16.0

8.0-9.0

2.50-4.00

2.50-1-4.00

1.00-2.00

1.00-2.00

 

 

Ta

Nb

C

Fe

 Zr

B

O

1.00-2.00

0.50-1.50

<=0.15

<=0.10

<=0.10

<=0.15

<=0.01

 

 